Posted by KB on April 11, 1999 at 08:59:07:
In Reply to: Re: Techniques on smoothing out weathered tin on 51 Farmall H posted by Dangit! The Red Again with pix on April 11, 1999 at 08:43:17:
Red: I always use a filling/surfacing primer to do what you describe. It requires multiple coats to build up and fill in all the blemishes. It is a lacquer based product and dries quickly. Sanding is a must between the coats to prevent excess buildup. Needs to be done after the metal has been cleaned and primed with a sealing primer. Looks like you have quite a bit of work.